Curing at room temperature should be carried out for 7 days in order to obtain full mechanical strength and within 14 days in order to achieve chemical resistance. During use, small portions of the composition should be prepared, which will be used within several minutes. The thickness of the poured layer in one process can not exceed 0.5 cm. Optimum working conditions are 20 ° C and relative humidity up to 65%. It is not recommended to make floors below 15 ° C. Higher humidity may cause cloudiness, cratering, stickiness on the cured coating. The reduction of the substrate temperature during curing below the dew point has a particularly critical effect on the appearance and quality of the coating. In the case of multi-layer coatings, the next layer can never be applied if the temperature of the substrate is lower than or equal to the dew point temperature.